Forensic Breakdowns: Aluminum to Copper Splices
Older & Historic Homes

Forensic Breakdowns: Aluminum to Copper Splices

Is this illegal wire connection secretly burning down your house?

This is a terrifying forensic breakdown of galvanic corrosion. When you twist copper and aluminum wires together without the proper dielectric compound, they chemically react and destroy each other. This code loophole from DIYers creates intense resistance and extreme heat. It is a material forensics nightmare that guarantees failure.

For professional, specialized remediation of aluminum wiring, contact the experts at CharmCityElectric.com.